Typical Magnetic Properties of Sintered Alnico Magnets |
|
Grade |
Residual
Induction(Br): mT(Gs) |
Coercive Force(Hcb): KA/m(Oe) |
Intrinsic Coercive Force(Hcj):
KA/m(Oe) |
Max. Energy
Product(BH)max: KJ/m3(MGOe) |
Density(D): g/cm3 |
Max. Operating Temp. (Tw):
°C |
Remark |
|
FLN8 |
520(5200) |
40(500) |
|
8-10 (1.0-1.25) |
6.8 |
450 |
Isotropic |
|
FLNG12 |
700(7000) |
40(500) |
43(540) |
12-14 (1.5-1.75) |
7.0 |
450 |
|
|
FLNGT14 |
570(5700) |
|
78(980) |
14-16 (1.75-2.0) |
7.1 |
500 |
|
|
FLNGT18 |
560(5600) |
|
90(1130) |
18-22 (2.25-2.75) |
7.2 |
500 |
|
|
FLNG28 |
1050(10500) |
|
47(590) |
28-33 (3.5-4.15) |
7.2 |
500 |
Anisotropic |
|
FLNG34 |
1100(11000) |
|
51(640) |
34-38 (4.3-4.8) |
7.2 |
500 |
|
|
FLNGT28 |
1000(10000) |
|
57(710) |
28-30 (3.5-3.8) |
7.2 |
500 |
|
|
FLNGT31 |
780(7800) |
|
106(1130) |
33-36 (3.9-4.5) |
7.2 |
500 |
|
|
FLNG33J |
650(6500) |
|
150(1880) |
31-36 (4.15-4.5) |
7.2 |
500 |
|
|
FLNGT38 |
800(8000) |
|
126(1580) |
38-42 (4.75-5.3) |
7.2 |
500 |
|
|
FLNGT42 |
880(8800) |
|
122(1530) |
42-48 (5.3-6.0) |
7.25 |
500 |
| Remarks: ● The above-mentioned data are given at room temperature. ● The Max. operating temperature will vary with L/D (Length to Diameter ratio), coating and environmental factors. ● If the material you are looking for is not listed, please contact us to discuss your needs. |
|